5G RRU RF Amplifier Heat Sinks: Copper, Tungsten-Copper or Aluminum? The Conductivity, Weight and Shielding Trade-off
Published:

5G RRU RF Amplifier Heat Sinks:
Copper, Tungsten-Copper or Aluminum? The Conductivity, Weight and Shielding Trade-off
There is no single right metal for a 5G RRU power amplifier, because the heat path is not one part. Aluminum owns the enclosure, the fin field and the cast carrier, where grams and cost per unit dominate and expansion is carried by the die-attach and the thermal interface. Tungsten-copper owns the die-level spreader and flange, where the joint has to survive repeated power cycles against GaN, GaAs or SiC. Pure copper sits between them, used where the heat flux is high and expansion is managed by the die-attach or by a compliant interface. An RRU commonly contains all three, at different nodes, chosen for different reasons.
Decide per thermal node, not per enclosure
Follow the heat from junction to air and the constraints change at every step. At the die, the limit is flux density and CTE mismatch across a solder or sinter joint a few tens of microns thick. At the spreader, it is lateral spreading of a small, very hot footprint into a larger area. At the carrier and housing, it is total thermal resistance to ambient, mass, wind load on a tower, and the cost of a die-cast tool.
| Material | Thermal conductivity (W/m·K) | CTE (ppm/K) | Density (g/cm³) | Match to GaN / SiC | Typical RRU node |
|---|---|---|---|---|---|
| Al 6063-T6 extrusion | ≈200 | ≈23 | 2.7 | Poor | Housing walls, fin field, brackets |
| Al A380 die cast | ≈95 | ≈22 | ≈2.7 | Poor | Integrated housings, low-flux blocks |
| Pure copper (C110) | ≈390 | ≈17 | 8.9 | Limited | High-flux spreaders, pedestals, heat-pipe bases |
| W70Cu30 | ≈190–210 | ≈9–11 | ≈14.0–14.3 | Good | Die-level spreader, PA flange |
| W80Cu20 | ≈170–190 | ≈8–8.5 | ≈15.2–15.6 | Better | GaN/SiC packages, CTE-critical lids |
Figures are indicative published ranges for wrought and powder-metallurgy grades (Refs. 1, 4); the governing values are those on the grade datasheet for the lot you buy, since copper content, porosity and impurity level all move conductivity, CTE and density.
Two numbers that decide the spreader
Through-plane conduction resistance of a plate is `R = t / (k · A)`. At fixed area, that term rises with thickness and falls with conductivity: moving from about 200 to about 390 W/m·K halves it, the same factor as halving thickness. Spreading from a small die footprint is a separate term. Extra thickness aids lateral conduction only while the plate is thin relative to the source; beyond that it mainly adds mass. A thin copper insert can therefore cut resistance at the die footprint, where the area is small and the flux is concentrated. Mass still follows density times volume, so copper at the footprint is the heavier insert, and extending the same swap to the full housing adds kilograms for little thermal return.
Bond displacement along a joint is `δ ≈ Δα · ΔT · L`. Against GaN near 5–6 ppm/K, aluminum near 23 ppm/K leaves a differential of about 17 ppm/K; W70Cu30 at 9–11 ppm/K cuts that differential by more than half. Over the same temperature swing and joint length, the aluminum joint therefore sees more than twice the shear displacement, taken up in a solder or sinter layer only tens of microns thick. That displacement is what cracked die-attach and delaminated lids track, and it is the reason to pay W-Cu prices at the die node. On the housing, no semiconductor is bonded, and a compliant thermal pad absorbs the movement.
Where aluminum still earns its place
Aluminum is the right metal above the spreader. Its specific heat is higher than copper's, so each kilogram stores more heat, which matters for transient peaks in TDD duty cycles, and it extrudes and die-casts into finned geometries that are costly to machine from copper. A tower-mounted RRU is also a mechanical structure: wind loading, ice load and mast capacity all scale with head weight, and a copper housing is a structural penalty the thermal gain does not repay.
Shielding follows the enclosure, not the spreader
EMI containment in an RRU is set by the housing, gasket joints and cable entry, and a well-sealed die-cast aluminum box does that job at low cost. What trips designs is surface finish: anodized aluminum is an insulator, so every gasket land and ground point needs masking, a conductive conversion coating or a plated insert. Copper and W-Cu parts plate readily with Ni or Au, which is why package-level lids and cavity covers are often specified in W-Cu — they combine a matched CTE with a conductive, solderable, bondable surface that closes the module cavity at the same time it spreads heat. Treat shielding as a joint-and-coating discipline and the material choice becomes a secondary question.
What MIM can hold, and where it fails
Metal injection molding fits the parts in the middle of this stack: micro-finned spreaders, thin-wall cavity covers, pedestals with integral mounting features, and near-net flanges that would otherwise be milled from bar. The failure modes are predictable. Non-uniform wall sections shrink at different rates, so a thick boss beside a thin fin is a cracking risk in debinding and sintering. Thick sections sinter to lower density than thin ones, which shows up as a conductivity difference that external dimensions do not reveal. Copper is oxygen-sensitive, and binder carbon has to be burned out cleanly; residual porosity lowers the conductivity the grade was chosen for. Housings on the scale of an RRU enclosure are castings or extrusions.
The practical design window is a part that fits in a palm, holds wall thickness within roughly 2:1 across its section, and needs its critical faces ground or milled after sintering to hit flatness and parallelism.
Evidence worth auditing before you commit a tool
Ask for the things that determine whether the promise survives production. On copper and W-Cu programs, look for sintered density reported per lot — Newlife - MIM runs pure copper, copper alloy and W-Cu MIM to a sintered density of at least 8.4 g/cm³ with relative density ≥98 %, and holds near-net tolerances of ±0.3 % to ±0.5 % before finish machining. Feedstock particle size sets the shrinkage curve: feedstocks made from the supplier's own ultrafine copper, iron and nickel powders at D50 ≤ 3 µm are the lot-control point to audit. W-Cu diffusion plates and heat sinks are produced from self-developed tungsten powder, can carry machined microchannels and mounting faces, and accept Ni/Au plating and soldering. For a qualified volume program, IATF 16949, ISO 9001 and ISO 14001 registration should be in the audit pack, alongside 20-plus sintering furnaces.
Next steps
Fix the node before you fix the metal: write down the flux density, the allowed junction temperature, the CTE of the device you are bonding to, and the mass budget for that node. That list eliminates two of the three candidates in most cases. Then prototype the surviving option in the actual stack, because interface material and flatness often dominate the remaining thermal resistance. Visit http://www.newlife.cn to review the copper, W-Cu and PM heat-spreader portfolio, and contact the Newlife - MIM application engineering team for a free consultation and a custom engineering proposal built around your RRU thermal stack.
References
1. ASM Handbook, Volume 7: Powder Metal Technologies and Applications. ASM International, 1998. 2. German, R. M. Sintering Theory and Practice. Wiley-Interscience, 1996. 3. MPIF Standard 35: Materials Standards for Metal Injection Molded Parts. Metal Powder Industries Federation. 4. Tummala, R. R. Fundamentals of Microsystems Packaging. McGraw-Hill, 2001. 5. JEDEC JESD51 series: Methodology for the Thermal Measurement of Component Packages. 6. Newlife New Materials Co., Ltd. — RF heat sink and thermal packaging product pages. http://www.newlife.cn